Panem, Muhammad Burhanudin (2016) Optimasi pemisahan TiO2 dari pasir besi pantai Sukabumi Selatan menggunakan proses leaching asam klorida dengan reduktor Fe0. Diploma thesis, UIN Sunan Gunung Djati Bandung.
|
Text (COVER)
1_COVER.pdf Download (210kB) | Preview |
|
|
Text (ABSTRAK)
2_ABSTRAK.pdf Download (296kB) | Preview |
|
|
Text (DAFTAR ISI)
3_DAFTAR ISI.pdf Download (495kB) | Preview |
|
|
Text (BAB I)
4_BAB I.pdf Download (205kB) | Preview |
|
Text (BAB II)
5_BAB II.pdf Restricted to Registered users only Download (432kB) |
||
Text (BAB III)
6_BAB III.pdf Restricted to Registered users only Download (313kB) |
||
Text (BAB IV)
7_BAB IV.pdf Restricted to Registered users only Download (597kB) |
||
Text (BAB V)
8_BAB V.pdf Restricted to Registered users only Download (195kB) |
||
Text (DAFTAR PUSTAKA)
9_DAFTAR PUSTAKA.pdf Restricted to Registered users only Download (427kB) |
Abstract
INDONESIA : Pasir besi merupakan salah satu bahan baku untuk memproduksi titanium dioksida karena mineral utama penyusunnya adalah magnetit (Fe3O4), ilmenit (FeTiO3) dan hematit (Fe2O3). Berdasarkan hasil karakterisasi dengan XRF (X-Ray Fluorescence) diketahui persentase TiO2 pada pantai Sukabumi Selatan sebesar 24,22 %. Pada penelitian ini TiO2 diperoleh dari estraksi pasir besi dengan metode leaching HCl di mana konsentrasi HCl dioptimasi yaitu 4 M, 6 M dan 8 M. sebelum dicampurkan dengan HCl, pasir besi ukuran 100 mesh melewati tahap pra-oksidasi yaitu dengan cara dikalsinasi pada suhu 700 °C. Campuran pasir besi dengan HCl dicampurkan serbuk Fe0 sebagai reduktor untuk meningkatkan oksidasi pada reaksi pengendapan TiO2. Berdasarkan hasil XRF produk leaching HCl disimpulkan bahwa konsentrasi HCl optimum adalah 6 M dengan persentasi TiO2 terbesar yaitu 76,73 %. ENGLISH : Iron sand can be the one of a raw material for producing titanium dioxide as the main constituent minerals are magnetite (Fe3O4), ilmenite (FeTiO3) and hematit (Fe2O3). Based on the results of characterization by XRF (X-Ray Fluorescence) known percentage of TiO2 in iron sand of South Coast Sukabumi is 24.22%. In this study, TiO2 obtained from extraction of iron sand by leaching using HCl which the concentration of HCl is optimized 4 M, 6 M and 8 M. before mixed with HCl, iron sand 100 mesh pass pre-oxidation stage that is by calcined at a temperature of 700 ° C , iron sand mixture with HCl and Fe0 powder as a reducing agent to enhance the deposition of TiO2 oxidation reaction. Based on the results of XRF on leaching HCl product concluded that the optimum concentration was 6 M HCl with the largest percentage of TiO2 is 76.73%.
Item Type: | Thesis (Diploma) |
---|---|
Uncontrolled Keywords: | TiO2; pasir besi; leaching; XRF.; |
Subjects: | Chemistry and Allied Science > Data Processing and Analysis of Chemistry Ecology > Environmental Chemistry |
Divisions: | Fakultas Sains dan Teknologi > Program Studi Kimia |
Depositing User: | rofita fita robi'in |
Date Deposited: | 04 Jul 2019 04:22 |
Last Modified: | 04 Jul 2019 04:22 |
URI: | https://digilib.uinsgd.ac.id/id/eprint/21208 |
Actions (login required)
View Item |